Cruisers Forum
 

Go Back   Cruisers & Sailing Forums > Engineering & Systems > Construction, Maintenance & Refit
Cruiser Wiki Click Here to Login
Register Vendors FAQ Community Calendar Today's Posts Log in

Reply
  This discussion is proudly sponsored by:
Please support our sponsors and let them know you heard about their products on Cruisers Forums. Advertise Here
 
Thread Tools Search this Thread Rate Thread Display Modes
Old 20-07-2017, 07:09   #1
Registered User
 
Davidhoy's Avatar

Join Date: Jul 2016
Location: West Palm Beach, FL
Boat: Catalina 470
Posts: 1,131
Does Loctite protect against galvanic corrosion?

I'm installing an aluminum arch kit on the stern of my boat. The aluminum parts fit snugly together and then are secured with stainless bolts going into tapped threads in the aluminum. The vendor recommends the use of Loctite on the threads. My question is, does Loctite provide any dissimilar-metal galvanic corrosion protection? If not, can anyone recommend a product that provides both thread locking and galvanic corrosion protection?

Thanks,
David.
__________________
Twenty years from now you will be more disappointed by the things that you didn't do than by the ones you did do. So throw off the bowlines. Sail away from the safe harbor. Catch the trade winds in your sails. Explore. Dream. Discover.” – Mark Twain
Davidhoy is offline   Reply With Quote
Old 20-07-2017, 07:10   #2
Registered User
 
SailRedemption's Avatar

Join Date: Feb 2014
Location: New Orleans
Boat: Kaufman 47
Posts: 1,184
Re: Does Loctite protect against galvanic corrosion?

It may, but tefgel is much better for that. If you don't need a thread locker then tefgel is the way to go. Apply liberally.
SailRedemption is offline   Reply With Quote
Old 20-07-2017, 07:46   #3
Registered User

Cruisers Forum Supporter

Join Date: May 2011
Location: Miami Florida
Boat: Ellis Flybridge 28
Posts: 4,069
Re: Does Loctite protect against galvanic corrosion?

I use Permatex #3 on stainless that is going into aluminum.

I learned that trick from an outboard mechanic who dealt with stainless bolts in aluminum every day. The first time he would work on an old engine, he had to use his fire wrench (torch) to get it apart. If it came back after he reassembled it with Permatex, he had no problem getting it apart.

It really prevents the stainless and aluminum from becoming one.
__________________
Retired from Hopkins-Carter Marine Supplies
HopCar is offline   Reply With Quote
Old 20-07-2017, 08:03   #4
Registered User

Join Date: Aug 2009
Location: between the devil and the deep blue sea
Boat: a sailing boat
Posts: 20,448
Re: Does Loctite protect against galvanic corrosion?

Which Loctite? They make a range of products. I believe one may be a corrosion inhibitor. But regular Loctites are those used as anti-seize and threadlock properties.

Tefgel, Duralac, Lanocote, etc. are good protectors. Tefgel and Lanocote work while Duralac hardens. But Duralac can be painted over. etc. All good stuff.

There are also other less globally common products.

So have your pick.

b.
barnakiel is offline   Reply With Quote
Old 20-07-2017, 08:38   #5
Registered User
 
UNCIVILIZED's Avatar

Join Date: Jun 2014
Location: Up the mast, looking for clean wind.
Boat: Currently Shopping, & Heavily in LUST!
Posts: 5,629
Re: Does Loctite protect against galvanic corrosion?

I tend to use Blue Loctite for this, with pretty good results. Including on fasteners in spars. And as an indicator of what some others think of it, Harken routinely ships their hardware with it. Hardware meaning the sort which has stainless fasteners going into aluminum parts. Many/most of which are quite structural, but that do need to be diassembled, including for routine maintenance.

That said, why not look it up yourself? This in addition to both calling & emailing them about it. That way you get multiple feedback channels. And if the concensus of it sounds good to you, then give it a go.

One other thought, is that normally when using Blue Loctite, such as to secure stainless to stainless, or on things outside of the marine environment. Is that you usually only use a drop or three of the stuff. But to get better galvanic isolation you'll want to coat more of the threads on a fastener, sometimes their entirety. But do a bit of testing of this technique on something non-critical first, as is wise to do with anything new.
__________________

The Uncommon Thing, The Hard Thing, The Important Thing (in Life): Making Promises to Yourself, And Keeping Them.
UNCIVILIZED is offline   Reply With Quote
Old 20-07-2017, 08:48   #6
Senior Cruiser

Cruisers Forum Supporter

Join Date: Aug 2009
Posts: 4,033
Re: Does Loctite protect against galvanic corrosion?

Mmmm. . . If you are putting stainless machine screws into aluminum, and you want them to come out later . . . You should use helicoils (or other threaded insert).

That is the only proper and sure way to achieve the objective.

Even with tuffgel, in my experience, 25-30% of the machine screws will be at least semi-frozen (after hard use/tough climates) 5 years later.

Put the helicoils in with locktite.
estarzinger is offline   Reply With Quote
Old 20-07-2017, 09:10   #7
Registered User
 
Cheechako's Avatar

Join Date: Aug 2006
Location: Skagit City, WA
Posts: 25,649
Re: Does Loctite protect against galvanic corrosion?

OP: I like lanolin. But of course that wont lock the screws in place. I doubt you will have an issue if you just keep an eye on the screws from time to time. If you have aluminum tubes that slip inside one another I would coat the mating area also, if Salt gets in there they may become unseparable.
__________________
"I spent most of my money on Booze, Broads and Boats. The rest I wasted" - Elmore Leonard











Cheechako is offline   Reply With Quote
Old 20-07-2017, 09:21   #8
Registered User
 
Davidhoy's Avatar

Join Date: Jul 2016
Location: West Palm Beach, FL
Boat: Catalina 470
Posts: 1,131
Re: Does Loctite protect against galvanic corrosion?

Quote:
Originally Posted by UNCIVILIZED View Post
I tend to use Blue Loctite for this, with pretty good results. Including on fasteners in spars. And as an indicator of what some others think of it, Harken routinely ships their hardware with it. Hardware meaning the sort which has stainless fasteners going into aluminum parts. Many/most of which are quite structural, but that do need to be diassembled, including for routine maintenance.

That said, why not look it up yourself? This in addition to both calling & emailing them about it. That way you get multiple feedback channels. And if the concensus of it sounds good to you, then give it a go.

One other thought, is that normally when using Blue Loctite, such as to secure stainless to stainless, or on things outside of the marine environment. Is that you usually only use a drop or three of the stuff. But to get better galvanic isolation you'll want to coat more of the threads on a fastener, sometimes their entirety. But do a bit of testing of this technique on something non-critical first, as is wise to do with anything new.
I just spoke with tech-support at Loctite, and they recommended Blue 243, and coating the entire bolt, except the exposed surface of the head. Basically it will provide thread-locking *AND* corrosion protection whenever it is between two mated surfaces. Looks like you had the right answer :-)

My other option, once the arch is fully installed, is to have someone come over and weld all the joins. I may actually consider this down the road...

Thanks,
David.
__________________
Twenty years from now you will be more disappointed by the things that you didn't do than by the ones you did do. So throw off the bowlines. Sail away from the safe harbor. Catch the trade winds in your sails. Explore. Dream. Discover.” – Mark Twain
Davidhoy is offline   Reply With Quote
Old 20-07-2017, 09:21   #9
Registered User

Join Date: Dec 2013
Posts: 23
Re: Does Loctite protect against galvanic corrosion?

I have used Never-Seize for decades and never had a galvanic problem. However, do NOT use copper based Never-Seize on aluminum. Use the nickel based stuff made for stainless. It's dark gray. It's also messy. But it works. The nickel based NeverSeize can be used on steel and other metals, too. I use it on bronze turnbuckles, shackle pins, just about everything you want to be able to disassemble.
wcapman is offline   Reply With Quote
Old 20-07-2017, 09:21   #10
Registered User
 
Davidhoy's Avatar

Join Date: Jul 2016
Location: West Palm Beach, FL
Boat: Catalina 470
Posts: 1,131
Re: Does Loctite protect against galvanic corrosion?

Quote:
Originally Posted by Cheechako View Post
If you have aluminum tubes that slip inside one another I would coat the mating area also, if Salt gets in there they may become unseparable.
Good point! Thanks!
__________________
Twenty years from now you will be more disappointed by the things that you didn't do than by the ones you did do. So throw off the bowlines. Sail away from the safe harbor. Catch the trade winds in your sails. Explore. Dream. Discover.” – Mark Twain
Davidhoy is offline   Reply With Quote
Old 20-07-2017, 09:27   #11
Registered User
 
S/V Alchemy's Avatar

Join Date: May 2008
Location: Nova Scotia until Spring 2021
Boat: Custom 41' Steel Pilothouse Cutter
Posts: 4,976
Re: Does Loctite protect against galvanic corrosion?

Quote:
Originally Posted by barnakiel View Post
Which Loctite? They make a range of products. I believe one may be a corrosion inhibitor. But regular Loctites are those used as anti-seize and threadlock properties.

Tefgel, Duralac, Lanocote, etc. are good protectors. Tefgel and Lanocote work while Duralac hardens. But Duralac can be painted over. etc. All good stuff.

There are also other less globally common products.

So have your pick.

b.
Those would be my top-three go-tos, as well. I like Duralac on the mast, Lanacote on turnbuckles and Permatex/Tefgel on machinery. I have a steel boat, so the topic comes up a fair bit.
__________________
Can't sail? Read about our travels at https://alchemyonpassage.blogspot.com/. Can't sleep? Read www.alchemy2009.blogspot.com for fast relief. Can't read? Avoid www.volumesofsalt.blogspot.com, because it's just personal reviews of sea books.
S/V Alchemy is offline   Reply With Quote
Old 20-07-2017, 09:43   #12
Senior Cruiser

Cruisers Forum Supporter

Join Date: Aug 2009
Posts: 4,033
Re: Does Loctite protect against galvanic corrosion?

Quote:
Originally Posted by UNCIVILIZED View Post
Harken routinely ships their hardware with it..
Just FYI, if using harken as a benchmark . . . Pretty much all their aluminum is hard anodized (the black coating) which greatly reduced corrosion, and if you look in the loaded threaded holes you will usually see threaded inserts. I just copied this from one of their product descriptions . . ."Bolt holes in the hardcoat-anodized 6061-T6 aluminum are threaded with stainless steel inserts to prevent corrosion around the stainless bolts. "
estarzinger is offline   Reply With Quote
Old 20-07-2017, 10:40   #13
Registered User
 
sailon46's Avatar

Join Date: Jun 2015
Location: Houston
Boat: Beneteau Sense 46
Posts: 361
Images: 2
pirate Re: Does Loctite protect against galvanic corrosion?

The Germans in the UBoats put on everything Vaseline to prevent corrosion and galvanic issues between dissimilar metals. Ive used it everywhere I can, no corrosion anywhere.
Ernie
sailon46 is offline   Reply With Quote
Old 20-07-2017, 10:57   #14
Registered User
 
UNCIVILIZED's Avatar

Join Date: Jun 2014
Location: Up the mast, looking for clean wind.
Boat: Currently Shopping, & Heavily in LUST!
Posts: 5,629
Re: Does Loctite protect against galvanic corrosion?

Quote:
Originally Posted by estarzinger View Post
Just FYI, if using harken as a benchmark . . . Pretty much all their aluminum is hard anodized (the black coating) which greatly reduced corrosion, and if you look in the loaded threaded holes you will usually see threaded inserts. I just copied this from one of their product descriptions . . ."Bolt holes in the hardcoat-anodized 6061-T6 aluminum are threaded with stainless steel inserts to prevent corrosion around the stainless bolts. "
Touche! Helicoils definitely can be handy. And I'm in agreement with coating the slip together aluminum joints with an agent to prevent them from seizing to themselves. Either that, or purposefully bond them together, much as is done when repairing or assembling spars using sleeves & fasteners. It's common to bolt & bond sections together when doing this.
__________________

The Uncommon Thing, The Hard Thing, The Important Thing (in Life): Making Promises to Yourself, And Keeping Them.
UNCIVILIZED is offline   Reply With Quote
Old 20-07-2017, 12:59   #15
Registered User

Join Date: Mar 2015
Location: San Francisco Bay area
Boat: Condor Trimaran 30 foot
Posts: 1,501
Re: Does Loctite protect against galvanic corrosion?

Vaseline...now that is common stuff and cheap. Thanks for the tip.
alansmith is offline   Reply With Quote
Reply

Tags
corrosion, rot


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
Protecting connections and plugs against corrosion DITB Electrical: Batteries, Generators & Solar 41 20-01-2017 12:54
Building an Effective Faraday Cage to Protect Against Lightning Strikes teneicm Marine Electronics 58 25-01-2012 18:50
Shore Power and Galvanic Corrosion scalleia Electrical: Batteries, Generators & Solar 7 21-07-2010 19:05
The Galvanic Series and Corrosion GordMay Construction, Maintenance & Refit 8 22-05-2010 10:26

Advertise Here


All times are GMT -7. The time now is 06:28.


Google+
Powered by vBulletin® Version 3.8.8 Beta 1
Copyright ©2000 - 2024, vBulletin Solutions, Inc.
Social Knowledge Networks
Powered by vBulletin® Version 3.8.8 Beta 1
Copyright ©2000 - 2024, vBulletin Solutions, Inc.

ShowCase vBulletin Plugins by Drive Thru Online, Inc.